Gold evaporation coating on silicon - thermal treatment
for adhesion
2008-05-10
MosheGold evaporation coating on silicon - thermal treatment
for adhesion
Moshe
Last week I asked about an adhesion coating achieved between gold and silicon. Since then I've heard about a different way to achieve that. I talked about thermal treatment so the gold coating absorb to the silicon, at that way the adhesion obtain with no third layer. The general thermal treatment recipe is heating to 400 Celsius degrees for few hours in inert environment. Has anyone done that before? Whet is the exact recipe for this treatment ? Thank you