Hi, Garret is right, an UV adhesive should work fine, but you could even try with a new SU-8 layer: spin coat SU-8 on the substrate cap (glass, PC,...), do the soft bake and put the cap over your device with the SU-8 layer in contact with your device, expose it to UV and finally do the hard bake again, you will get a nice transparent cap. I hope it helps Eowin > -----Original Message----- > From: seyeda@ualberta.ca [mailto:seyeda@ualberta.ca] > > Sent: Friday, May 09, 2008 1:10 PM > To: General MEMS discussion > Subject: [mems-talk] Material for capping a SU8-2050 > Microfluidic > Opto-BioChip > > Hi all, > > I have made a microfluidic Opto-Biochip in SU8 2050 > on a glass > substrate. > Now I need to cap this with another optically clear > material such as > glass, PDMS, PMMA or any other material that may do > the job. Up to now > we haven't had success in bonding any of these > materials to SU8 after > post exposure bake. Does anybody know a material and > the process that > may work as a cap for SU8 chip.