Does ultrasonic damage metal film during lift-off?
2010-03-16
Li. Zhang2010-03-16
Harsh Sundani2010-03-17
mikas remeika2010-03-17
Bill Moffat2010-03-18
Enrique San Andrés Serrano2010-03-25
Li. ZhangDoes ultrasonic damage metal film during lift-off?
Harsh Sundani
Hi Li, I have successfully lifted-off metal films of similar thickness by a 20-30 min ultrasonic dip. I don't think it will damage the film. Regards, Harsh Sundani Graduate Research Assistant, University of Toledo, Toledo, Ohio. > Date: Mon, 15 Mar 2010 23:20:29 -0400 > From: anli5210@gmail.com > To: mems-talk@memsnet.org > Subject: [mems-talk] Does ultrasonic damage metal film during lift-off? > > Hi all, > > I'm doing lift-off using ultrasonic bath after soak my samples in NMP > overnight. However, some parts are difficult to be lifted off. > Thus, I increased the ultrasonic cleaning duration. But I'm afraid a long > ultrasonic cleaning (20-30min) might damage the metal film which is 150nm > sputtered Al. > > Would that be a problem? > > Thanks, > > Li. Zhang