[MEMS-Business] Float Zone , High resistivity and other specialty Silicon

Ken Smth kasmith2 at ix.netcom.com
Tue Oct 16 18:46:56 EDT 2007


If you have a need for SOi Wafers, Float Zone or other high resistivity or low oxygen silicon wafers or need some specialty thick or very thin wafers please contact Kmbh Technologies. We also supply CZ wafers as well as quartz , glass and other materials. 

Ken Smith 
47 Rocket Circle 
Rancho Cordova, CA 95742 USA
ph 510 714 5055  fax 510 217 4421
emailto:kasmith2 at ix.netcom.com