One trick that Dow recommends for its Sylgard 184 is a mold release agent. I
think in reality it's a cure inhibitor. It's a 1 or 2% (by volume) solution
of Liquinox. You dip your substrate in that solution and let it air dry.
Then apply the PDMS.
In theory this should work for a wide variety of substrates.
Bill Eaton, Ph.D.
Materials & Analysis Manager
NP Photonics
5706 Corsa Avenue, Suite 100
Westlake Village, CA 91362
Voice: (818) 991-7044 x211
eFax: (503) 214-5559
mailto://bill@npphotonics.com
www.parvenutech.com
> -----Original Message-----
> From: mems-talk-admin@memsnet.org
> [mailto:mems-talk-admin@memsnet.org]On
> Behalf Of Zhizhong Yin
> Sent: Wednesday, November 06, 2002 7:53 AM
> To: mems-talk@memsnet.org
> Subject: [mems-talk] Material for PDMS mold
>
>
>
>
> hi, everyone,
>
> Does anybody know what material is good for PDMS mold?
> I want to make a very thin structure by PDMS, so I am looking for a
> material for the mold which will not bond with PMDS tightly.
> In this way I
> can peel off my PDMS structure from the mold without hurting it.
> Thanks
>
> Zhizhong Yin
> Phone#: 410-516-8525(o) Johns Hopkins University
> 410-662-4760(h) 200 Latrobe Hall
> email:zzyin@titan.me.jhu.edu 3400 N. Charles Street
> homepage:www.me.jhu.edu/~zzyin Baltimore MD 21218
> ***********************************************************
>
>
>
>
> _______________________________________________
> MEMS-talk@memsnet.org mailing list: to unsubscribe or change your list
> options, visit http://www.memsnet.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/
>
More information about the MEMS-talk
mailing list