[mems-talk] Ti Etch

Rick Morrison rmorrison at radantmems.com
Wed Jul 2 08:52:15 EDT 2003


Hi,

You can try 10% HF or I like to use 98% H2O2/2% NH4OH.

Rick


-----Original Message-----
From: mems-talk-bounces+rmorrison=radantmems.com at memsnet.org
[mailto:mems-talk-bounces+rmorrison=radantmems.com at memsnet.org]On Behalf
Of kris
Sent: Tuesday, July 01, 2003 11:49 AM
To: General MEMS discussion
Subject: [mems-talk] Ti Etch



Dear all,

I am trying to etch Ti(300 Angs),which has aluminum
layer underneath it.I have used TiW-30 (25-40C)from
transene.I could see that after some time the Ti etch
rate reduces completely and etch almost stops.I think
due to the formation of Tio2 the etch rate drops.

Can anyone suggest me a good Titanium etchant that
should not attack Al.

Your suggestions are highly helpful.
Thanks
Kris

__________________________________
Do you Yahoo!?
SBC Yahoo! DSL - Now only $29.95 per month!
http://sbc.yahoo.com

_______________________________________________
MEMS-talk at memsnet.org mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/



More information about the MEMS-talk mailing list