[mems-talk] Mumps structure length prevent stiction
weiwei2
weiwei2 at pd.jaring.my
Thu Jul 3 00:09:22 EDT 2003
using poly2 only, i achieve 1000um without initial stiction. But some does
stick after actuated few times
Leow
Universiti Teknologi Malaysia
----- Original Message -----
From: "rakesh babu" <rocky_mems at yahoo.com>
To: <mems-talk at memsnet.org>
Sent: Wednesday, July 02, 2003 10:35 AM
Subject: [mems-talk] Mumps structure length prevent stiction
> hi all,
>
> I am designing structures using Mumps process .
>
> what is the maximum length of cantilever and bridge type structures
using both poly1
> and poly2 layers so that stiction does not occur.
>
> thank you so much for the help.
>
> regards,
> rakesh.
>
>
>
>
> ---------------------------------
> Do you Yahoo!?
> SBC Yahoo! DSL - Now only $29.95 per month!
> _______________________________________________
> MEMS-talk at memsnet.org mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/
More information about the MEMS-talk
mailing list