[mems-talk] Cu Metal Etchant
Greg Reimann
gjreiman at bu.edu
Wed Jul 2 13:15:19 EDT 2003
DA Nanomaterials sells a CMP slurry for copper. Don't know how you
would use it to pattern anything though.
Transene sells etchants for just about everything including copper.
You will need an adhesion layer especially if you are going to polish
it. Ti is working better for me than chrome, but I am trying to get
them both to work.
Greg Reimann
Boston University
-----Original Message-----
From: mems-talk-bounces at memsnet.org
[mailto:mems-talk-bounces at memsnet.org] On Behalf Of ÀÌÅ¿ø
Sent: Wednesday, July 02, 2003 11:01 AM
To: mems-talk at memsnet.org
Subject: [mems-talk] Cu Metal Etchant
hi.
I heard about Cu could be patterned by something like CMP Process (
damascene(?) process)
Are there any wet etchants fot Cu etch? If not, what is the main reason
about that?
Furthermore, Adhesion layer (Ti or Cr) is not required when I deposit Cu
on Si Wafer ?
Thank you for in Advance.
TW Lee.
-----------------------------------------------------------
AeroMEMS Laboratory.
School of Mechanical & Aerospace Engineering.
Seoul National University , Seoul , KOREA.
_______________________________________________
MEMS-talk at memsnet.org mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.