[mems-talk] Making holes in Pyrex glass wafers?
Tomblin, Graham (OH32)
Graham.Tomblin at Honeywell.com
Thu Jul 3 11:12:10 EDT 2003
Try www.bullen-ultrasonics.com
Regards Graham
-----Original Message-----
From: Gautham Viswanadam [mailto:absara at singnet.com.sg]
Sent: Wednesday, July 02, 2003 9:17 PM
To: General MEMS discussion
Subject: [mems-talk] Making holes in Pyrex glass wafers?
Hi, We are looking for supplier who can drill more than 1 mm holes on thick
(1 mm) Pyrex glass wafers. Please write to propak at singnet.com.sg Regards.
----- Original Message -----
From: "???" <twlee at aerojet.snu.ac.kr>
To: <mems-talk at memsnet.org>
Sent: Wednesday, July 02, 2003 11:01 PM
Subject: [mems-talk] Cu Metal Etchant
> hi.
>
> I heard about Cu could be patterned by something like CMP Process (
damascene(?) process)
>
> Are there any wet etchants fot Cu etch? If not, what is the main reason
about that?
>
> Furthermore, Adhesion layer (Ti or Cr) is not required when I deposit Cu
on Si Wafer ?
>
> Thank you for in Advance.
>
> TW Lee.
>
> -----------------------------------------------------------
> AeroMEMS Laboratory.
> School of Mechanical & Aerospace Engineering.
> Seoul National University , Seoul , KOREA.
> _______________________________________________
> MEMS-talk at memsnet.org mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/
_______________________________________________
MEMS-talk at memsnet.org mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/
More information about the MEMS-talk
mailing list