For most microelectronics applications, people tend to use single side
polished (SSP) wafers. These are wafers with a mirror finish on one side and
a rougher, lapped or etched surface on the other side. Double side polished
(DSP) wafers have a mirror finish on both sides. They are useful for certain
MEMS processes that require doing operations on both sides of the wafer.
Most photolithographic processes and many deposition processes will not
yield very good results on the rough side of an SSP wafer. Furthermore,
processes that require front to backside alignment typically rely on using
an infrared camera to see through the wafer to see a pattern. The rough side
of an SSP wafer typically is too great for IR alignment.

Regards,

Bill Eaton, Ph.D.
Materials & Analysis Manager
NP Photonics

> -----Original Message-----
> From: mems-talk-bounces at memsnet.org
> [mailto:mems-talk-bounces at memsnet.org]On Behalf Of Tom Fan
> Sent: Wednesday, July 02, 2003 12:17 PM
> To: mems-talk at memsnet.org
> Subject: [mems-talk] DSP vs SSP
>
>
>
>
> Wafers have two polishing options: Double Side Polished or
> Single Side
> Polished. I am wondering whats the particular applications
> for these two types
> of wafers? Why are they differentiated?
> Anybody could enlighten me?
>
> Thanks,
> Tom Fan
>
>
> _______________________________________________
> MEMS-talk at memsnet.org mailing list: to unsubscribe or change your list
> options, visit
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/




More information about the MEMS-talk mailing list