We have some surplus 3" & 4" high resistivity silicon wafers.
4" (100),FZ, N(Pho), R = 10k ~ 100k ohm-cm, thickness = 900+/-25 um, single side polish,
250nm thermal SiO2 on top, Mfg = International wafer service, qty = ~ 100 ea.,
3" (100) FZ, N(pho), R = 1k ~ 4k, thickness = 600+/- 25 um, single side polish,
Mfg = Topsil, qty = 200 ea.,