I do not recommend evaporation method.
As platinum melting temperature is very high and vapor
pressure is very low even at Au melting temperature,
SU-8 layer could be easily burned by high temperature
of evaporator temperature.
Try sputtering.
Regards,
Sokwon Paik
--- Kirt & Erika Zipf-Williams
<zipf-williams at mindspring.com> wrote:
> > Good day everyone,
> > I am a research student in U.K.
> > Could anyone please tell me wome ways i can
> deposite platinum film on
> SU-8?
> > Any suggestions are welcomed.