AW: [mems-talk] Protect backside of Si wafer from TMAH
nga
nga at katana.dimes.tudelft.nl
Tue Jul 8 18:16:23 EDT 2003
Yes,
It is possible. We use a home-made stainless steel holder like ammt and it
work well all the time.
>hi all,
>I need a wafer holder, too.
>
>My requriement is to protect the back and the edge of the wafer
>but without leaving an residuals an the front side.
>I couldn't figure out whether it is possible with the recommended wafer
>holders.
>
>regards
>Michaela
>
>>-----Ursprungliche Nachricht-----
>>Von: Bill Flounders [mailto:bill at eecs.berkeley.edu]
>>Gesendet: Montag, 7. Juli 2003 18:21
>>An: General MEMS discussion
>>Betreff: Re: [mems-talk] Protect backside of Si wafer from TMAH
>>
>>
>>Take a look at:
>>http://www.ammt.de/html/wafer_holders.html
>>
>>Bill Flounders, Ph.D.
>>Technology Manager
>>Berkeley Microlab
>>
>>
>>Pimpin Alongkorn wrote:
>>> Dear Folk,
>>>
>>> I would like to purchase a wafer holder for wet etching that can protect
>>> a backside of wafer from etchant solution such as HF, TMAH and KOH.
>>> Could you recommend me a Japan company (or other countries are O.K.)? It
>>> will be invaluable help for me. Thank you very much.
>>>
>>> Alongkorn Pimpin
>>> THT laboratory
>>>
>>> _______________________________________________
>>> MEMS-talk at memsnet.org mailing list: to unsubscribe or change your list
>>> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>>> Hosted by the MEMS Exchange, providers of MEMS processing services.
>>> Visit us at http://www.memsnet.org/
>>
>>
>>
>>
>
>
>_______________________________________________
>MEMS-talk at memsnet.org mailing list: to unsubscribe or change your list
>options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>Hosted by the MEMS Exchange, providers of MEMS processing services.
>Visit us at http://www.memsnet.org/
>
>
============================================================================
Nga. P.Pham, Ph.D
Delft University of Technology
Faculty of Electrical Engineering, Mathematics and Computer Science (EEMCS)
Delft Institute of Microelectronics and Submicrontechnology (DIMES)
Laboratory of Electronic Components, Technology & Materials (ECTM)
Feldmannweg 17
P.O Box 5053
2600 GB DELFT
THE NETHERLANDS
phone ++31-15-2781237
fax ++31-15-2622163
e-mail nga at dimes.tudelft.nl
homepage: http://www.dimes.tudelft.nl http://ectm.et.tudelft.nl
============================================================================
More information about the MEMS-talk
mailing list