> Hi Derek,
> Either matel will make a fine adhesion layer. Of the Cr and Ti, Ti tends
> to have a lower stress, but it is susceptible to HF.
>
> Jesse Fowler
> UCLA/MAE Dept., 420 Westwood Plaza, Room 37-129, ENGR IV
> Los Angeles, CA 90095-1597 | (310)825-3977
> "Observations of nature, no matter how seemingly arcane, are like
> peeling off one more layer from the great onion of knowledge"
> -- Don Petit, ISS science officer
>
> On Mon, 7 Jul 2003, Chen-Han Lee wrote:
>
> > Hi everyone,
> >
> > thank you all especially Kirk and Bob,
> > you mention a adhesive layer for sputter platinum on silicon wafer
> > what material should i use? Will Ti or Cr do the job?
> > One more question, can i sputter gold on silicon wafer?
> >
> > Derek
> > 7/7/03
> >
> > ----- Original Message -----
> > From: "Kirt & Erika Zipf-Williams" <zipf-williams at mindspring.com>
> > To: "General MEMS discussion" <mems-talk at memsnet.org>
> > Sent: Thursday, July 03, 2003 7:25 PM
> > Subject: Re: [mems-talk] platinum on SU-8
> >
> >
> > > > Good day everyone,
> > > > I am a research student in U.K.
> > > > Could anyone please tell me wome ways i can deposite platinum film
on
> > > SU-8?
> > > > Any suggestions are welcomed.
> > > > Thank you for your time.
> > > > Chen-Han Lee
> > >
> > > You can sputter or evaporate platinum.
> > > Don't forget to use an adhesion layer.
> > >
> > > --Kirt Williams, Ph.D. consultant
> > >
> > >
> > > _______________________________________________
> > > MEMS-talk at memsnet.org mailing list: to unsubscribe or change your list
> > > options, visit
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> > > Hosted by the MEMS Exchange, providers of MEMS processing services.
> > > Visit us at http://www.memsnet.org/
> > >
> >
> >
> > _______________________________________________
> > MEMS-talk at memsnet.org mailing list: to unsubscribe or change your list
> > options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> > Hosted by the MEMS Exchange, providers of MEMS processing services.
> > Visit us at http://www.memsnet.org/
> >
>
>
> _______________________________________________
> MEMS-talk at memsnet.org mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/
>
More information about the MEMS-talk
mailing list