Laurell.com makes an inexpensive table top spinner.

-----Original Message-----
From: Sampo Tuukkanen [mailto:sampo.tuukkanen at phys.jyu.fi]
Sent: Wednesday, May 07, 2003 11:26 AM
To: MemsTalk
Subject: [mems-talk] Cheap Resist Spinner...


Hi!

I just broke our fotoresist spinner and...Ok, it was broken when I went to
clean room...

Does anyone know, where I could supply relatively cheap manual R&D resist
spinner?
It can be second-hand or new.

- Sampo Tuukkanen

_______________________________________________________
Sampo Tuukkanen, Room K215, Department of Physics,
PB 35 (YFL), FIN-40014 University of Jyväskylä, FINLAND
E-mail: sampo.tuukkanen at phys.jyu.fi
Tel: +35814 260 2392, Fax: +358 14 260 2351


_______________________________________________
MEMS-talk at memsnet.org mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/



More information about the MEMS-talk mailing list