[mems-talk] thermal evaporation of nickel

K. Winglee chatdevoile at yahoo.com
Mon Aug 7 15:49:34 EDT 2006


Hi,
  I am trying to deposit nickel using a thermal evaporator. I am using nickel powder. However, the nickel does not always evaporate off the boat. Does anyone have any suggestions on how to get the nickel to deposit?
  Thanks,
  Kathryn Winglee
  Undergraduate
  University of Washington