[mems-talk] Dicing Tape

walter essinger walter at elume.com
Mon Aug 7 18:21:25 EDT 2006


I am curious can you share the dimension of the smallest holes.
Are they less tha 50-75 mirons.,we have problems making them
Thanks
Walter
----- Original Message ----- 
From: "Mac McReynolds" <Mac.McReynolds at caliperls.com>
To: <mems-talk at memsnet.org>
Sent: Friday, August 04, 2006 8:01 AM
Subject: [mems-talk] Dicing Tape

> I'm going to be running some trials with highly polished glass substrates 
> full of through holes.  I find many vendors who offer "High Tack" UV 
> dicing tape, but they all seem to use different units and methods of 
> characterizing adhesion.  Can anyone in the group save me the trouble of 
> running a test matrix and recommend the highest tack tape from practical 
> experience.
>


More information about the MEMS-talk mailing list