[mems-talk] need sample holder for small chips in the pirahan clean

Florian Herrault fh59 at mail.gatech.edu
Wed Aug 16 11:26:57 EDT 2006


make your own teflon basket

Quoting Jing Xue <rainxj at gmail.com>:

> Hello,
>
> I also need sample holders for small chips (5mm x5mm, or smaller), but
> that is for holding chips in the sink of pirahan clean.
>

--
Florian Herrault, PhD student