Hi,
You can etch through by wet etching 'conc HF etching. You can check the
journal papers by Dr. Ciprian Illiscue by IBN, Singapore. I think its
published in Surface and Coating.
Thanks,
Pradeep
On 12/13/06, Shay Kaplan <shay at mizur.com> wrote:
>
> Gareth,
> ECD does work but the yields is very low, especially in thin wafers - they
> crack once you make the last hole!
>
> Shay
>
> -----Original Message-----
> From: mems-talk-bounces at memsnet.org [mailto:mems-talk-bounces at memsnet.org]
> On Behalf Of Gareth Jenkins
> Sent: Wednesday, December 13, 2006 4:03 PM
> To: General MEMS discussion
> Subject: Re: [mems-talk] etch through hole on pyrex glass
>
> You could try electrochemical discharge machining (also known as spark
> erosion).
> I believe two Japanese researchers, Shoji and Esashi, published work on
> this
> a while back, although I can no longer find the reference.
>
>
> _______________________________________________
> Hosted by the MEMS and Nanotechnology Exchange, the country's leading
> provider of MEMS and Nanotechnology design and fabrication services.
> Visit us at http://www.mems-exchange.org
>
> Want to advertise to this community? See http://www.memsnet.org
>
> To unsubscribe:
> http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>
More information about the MEMS-talk
mailing list