Dear All,
I woulkd like to know if there is any procedure similar to the bonding of
PDMS to glass to bond ITO-coated glass to PDMS. I would be greatful for the
suggestions.
The other problem is, i would like to make PDMS gels of variable young's
modulus. I have tried varying the composition of crosslinker to base
polymer for the Sylgard-184 kit. The problem i faced while doing this is
that the gel that is formed is very sticky due to the the uncured PDMS
oligomers. I would be grateful if someone suggests me to overcome this
problem or suggest a new method for making soft gels.
Thanking you,
--
V.S.Sri Kalyan.B
e-mail:- srikalyan at chemeng.iisc.ernet.in
ME, CHemical Engineering,
Indian Institute of Science,
Bangalore-12.
CELL1:9246546995
CELL2:9986704699