Hi all, i prepared 500ml of fresh BHF 1:4 and etched 50 nm of silicon
nitride from the entire surface of a 4'' silicon wafer. At the end of the
etch i noticed the formation of a salt which covered the entire silicon
wafer. In previous etch in the same conditions it never appared. What could
it be :o ?

Best regards,
Andrea