GARCIA BLANCO Sonia
Sonia.Garcia.Blanco at ino.ca
Fri Dec 15 11:00:53 EST 2006
Hi Barbara,
I had some time a similar problem and the conclusion was that the hotplate temperature was not completely uniform!. Maybe that is also producing your layer not to be perfectly baked (it should be hard after baking).
Good luck!
Sonia.
-----Message d'origine-----
De : Barbara Cortese [mailto:KORTESEB at libero.it]
Envoyé : Thursday, December 14, 2006 8:41 AM
À : mems-talk
Objet : [mems-talk] Su8-2100 soft bake
Dear all
Recently we met a problem using SU-8 2100. When spinning (at 1000rpm),after softbake treatment, waves appear on the layer. The hotplate I use is levelled, and I am using as a substrate silicon. The soft bake lasts 15 minutes at 65°and 60 min at 95°. I tried longer times of soft bake but the problem is always the same, and the layer is always soft.
Can you help me to solve this problem? What do you think the problem is caused by?
Barbara Cortese
------------------------------------------------------
Passa a Infostrada. ADSL e Telefono senza limiti e senza canone Telecom
http://click.libero.it/infostrada14dic06
**********************************************************************************
Ce courrier électronique s'adresse uniquement à la personne désignée
ci-dessus, il est confidentiel et ne doit pas être remis à une autre
personne, ni reproduit et son contenu ne peut être autrement divulgué..
Si ce courrier électronique vous est transmis par erreur, veuillez
nous en avertir immédiatement à l'adresse securite at ino.ca. Nous
vous remercions de votre collaboration.
This email is directed in confidence solely to the person named above,
and may not otherwise be distributed, copied or disclosed. If you have
received this email by error, please notify us immediately by email to
address security at ino.ca. Thank you for your cooperation.
**********************************************************************************
More information about the MEMS-talk
mailing list