Thank you for reply
I really need a Polycarbonate and its proper solvent.
The problem is that I can't make a solution with PC and Toluene(or PGMEA).
So, I am looking for good solvent which dissolve the PC well, or lower
Molecule weight of PC so that it sould be dissolved in Toluene or
PGMEA.
Thank you
On 12/20/06, neal at zbzoom.net <neal at zbzoom.net> wrote:
> Dear Stefano,
>
> What are you trying to do and does it have to be polycarbonate? I have
> some other sources that may provide different MW than you have tried.
>
> There are many solvents to use but what problems do you have when you use
> toluene or the other solvent you mentioned?
>
> There are many different polymers to use also so this is why I question
> you? I can possibly help.