[mems-talk] SU-8 Adhesion with SiO2
Prakash Mukre
prakash.mukre at gmail.com
Thu Dec 21 12:00:13 EST 2006
Hi All,
I am trying to deposit SU-8 over thermal oxide. SU-8 is part of the
final device I am fabricating, so I want it to adhere to the substrate
strongly. But with my current recipe SU-8 delaminates after
development. Following are the some process specs I am following.
SU-8 2100 Thickness: 200-250um
Softbake: 15min @65C, 100min @95C.
UV Dose: I have tried 400mJ/cm2 to 1000mJ/cm2
Hard Bake: 5min @65C, 20min @ 95C.
Development time: 10-20min.
I have tried using primers like HMDS, P20. Also I have tried using
Omicoat. What could be the possible reason for this? or SU-8 does not
adhere to thermal oxide at all?
Thanks,
Prakash