Hello Madhav,
You can purchase an electroless nickel plating kit, a company called
Transene used to sell this but, I am not sure if they still do. The
kits are relatively inexpensive.
The adhesion to PMMA may present an issue however I am not sure of this.
If you would like to contact me directly please feel free to do so.
Best Regards,
Seth Burtner
SBurtner at Filmtronics.com
-----Original Message-----
From: mems-talk-bounces at memsnet.org
[mailto:mems-talk-bounces at memsnet.org] On Behalf Of madhav rao
Sent: Thursday, November 02, 2006 7:48 PM
To: General MEMS discussion
Subject: [mems-talk] Nickel electroless Plating!!
Hi All,
I am not able to find a simple way of doing
electroless Nickel plating on PMMA patterned silicon
wafer. Can any one provide me any PDF file or any
procedure to do Electroless Nickel plating.