[mems-talk] How to clean single crystal TiO2 with chemicals?

VS Bhat vsbhat at sitarindia.com
Sat Nov 4 03:43:59 EST 2006


Dear Mr.Xiaojing,
H2O2 and HF or HNO3 and HF mixtures are generally used for Ti etching. May be
one of them can be tried if their use is not a problem in you case
Bhat
Quoting Xiaojing Zou <Xiaojing_Zou at brown.edu>:

> Hi:
>
>     Is there anybody having experience with wet etching single crystal TiO2
> substrate??? I want to etch the surface for half micron deep.  I tried H2SO4
> and HF, but it does not do the job. But as far as I know, acid will attach
> TiO2.
>
>    I do not quite understand why it is so hard to etch single crystal
> materials??


More information about the MEMS-talk mailing list