[mems-talk] temporary bonding solutions
ssood
ssood at hargray.com
Mon Nov 6 13:52:04 EST 2006
Sebastian,
Mitsui Chemicals sells water soluble tapes ( sold under trade name ICROS)
which should work for you. These tapes are soluble in water and are
excellent for temporary wafer bonding. You don't need heat or any other
solvents for removal.
Sumant Sood
Belford Research Inc.
-----Original Message-----
From: mems-talk-bounces at memsnet.org [mailto:mems-talk-bounces at memsnet.org]
On Behalf Of Mathieu Foquet
Sent: Monday, November 06, 2006 12:27 PM
To: Sebastian Sosin; mems-talk at memsnet.org
Subject: RE: [mems-talk] temporary bonding solutions
Revalpha thermal release tape is one idea. (Nitto Denko)
-----Original Message-----
From: mems-talk-bounces at memsnet.org
[mailto:mems-talk-bounces at memsnet.org] On Behalf Of Sebastian Sosin
Sent: Sunday, November 05, 2006 7:54 AM
To: mems-talk at memsnet.org
Subject: [mems-talk] temporary bonding solutions
I am looking for a temporary bonding solution that can be removed without
solvents (heat, UV.). It may be glue or adhesive tape. Does anyone know any
products like this?
More information about the MEMS-talk
mailing list