> Hi Every one,
> I am trying to do a diffusion study of flourescent dye through mems
> structure. I want to make a time vs diffusion profile and see how
> flourescent dye enters into mems structure with passage of time. My
> microstructures are SU8 and are made through conventional
> Photolithography.
> I ve been trying hard to diffuse flourescent dyes into my microstructures
> but I havent succceeded so far.
> Can Any one give me some idea??
> thanks in advance
--> Hi Ali
What do you mean by haven't succeeded?
Do you mean you haven't had any diffusion? or Do you mean you couldn't
measure diffusion although there is diffusion?
If you want contact me biomems at gmail.com