[mems-talk] Polymerisation of PDMS
Matthew Davies
m.davies at herts.ac.uk
Tue Oct 3 12:35:32 EDT 2006
60 deg C and 4 hours are the standard conditions I use.
Matt
University of Hertfordshire
-----Original Message-----
From: RABBIA Laurent [mailto:laurent.rabbia at recif.com]
Sent: Tuesday, 3 October 2006 8:26 AM
To: 'mems-talk at memsnet.org'
Subject: [mems-talk] Polymerisation of PDMS
Hello everybody,
Please, someone can tell me which is the temperature and time for complete
polymerisation of PDMS ? I know there is many process on it but in your
opinion which is the best ?
Reed you, Laurent.
--
No virus found in this outgoing message.
Checked by AVG Free Edition.
Version: 7.1.407 / Virus Database: 268.12.12/461 - Release Date: 2/10/2006
More information about the MEMS-talk
mailing list