Hi Guys I am trying to make an electrical contacts (four probe measurent) on organic samples. I am thinking to make chips with Pt and use FIB to make electrical contact. I can't use the lithography because the organic samples dissolve on Acetone. anyone has better idea? Hope to hear from you Thanks JP