[mems-talk] To remove Al layer from PMMA/glass substrate
Mathieu Foquet
mfoquet at pacificbiosciences.com
Mon Oct 16 17:48:16 EDT 2006
Did you consider something like espacer by showa denko? It is a conductive water-soluble polymer.
Mathieu
________________________________
From: mems-talk-bounces at memsnet.org on behalf of Hyunsoo Park
Sent: Sun 2006-10-15 11:39 PM
To: General MEMS discussion
Subject: Re: [mems-talk] To remove Al layer from PMMA/glass substrate
Thank you for reply.
I can't use gold right now. could anyone tell the solution to remove
Al layer without any damage to PMMA?
Otherwise, could anyone tell me another way to use glass substrate in
E-beam lithography?
Thank you.
More information about the MEMS-talk