[mems-talk] polyimide (Yogendra Yadav_04322601)

Lung-hao Hu lung.hu at colorado.edu
Wed Oct 18 12:33:39 EDT 2006


I used PI 2723 to fabricate a humidity sensor before.
Also you can try SU-8 2000.5 whose water absorption is 85% and dielectric
constant is 3.2.
It is good to be measured the capacitance change.

Lung-hao Hu