AW: [mems-talk] Anyone know what this thing called and where to buy
itfrom? Chip carrier? Chip bonding packaging pad?
Erik Jung
erju at izm.fhg.de
Thu Oct 19 09:32:13 EDT 2006
This is a old fashioned PinGridArray (PGA).
Check out Kyocery, NTK Tech or GlobalChipMaterials for supplies.
Regards,
Erik
-----Ursprüngliche Nachricht-----
Von: mems-talk-bounces at memsnet.org [mailto:mems-talk-bounces at memsnet.org] Im
Auftrag von Guangchi Archie Xuan
Gesendet: Donnerstag, 19. Oktober 2006 04:08
An: General MEMS discussion
Betreff: [mems-talk] Anyone know what this thing called and where to buy
itfrom? Chip carrier? Chip bonding packaging pad?
Hi, All,
I found out these two little ceramic-based chip carrier thingies
but nobody around me knows what it's called. I spent an hour googling but to
no avail. This is the thing that you can put your chip on wire bond the
electrical connection to the gold pads on the ceramic carrier and connects
to the outside using the pins at the bottom of the carrier.
I shot a few photos of them and put them here. If you can spend a
few seconds seeing the photo and let me know what they are called and where
I can buy them from.
More information about the MEMS-talk
mailing list