[mems-talk] contact angle measurement equipment needed
Bill Moffat
BMoffat at yieldengineering.com
Fri Sep 1 10:47:09 EDT 2006
Try manufacturing your own. Put a drop of water on a surface shine a
collimated light say a microscope light at it collect the shadow image
on a wall and measure the angle. Bill Moffat
-----Original Message-----
From: mems-talk-bounces at memsnet.org
[mailto:mems-talk-bounces at memsnet.org] On Behalf Of amron gary
Sent: Thursday, August 31, 2006 5:05 PM
To: General MEMS discussion
Subject: [mems-talk] contact angle measurement equipment needed
Hello:
I need a contact angle measurement equipment. Used or new? Plz contact
me on my email. Thanks
Gary