[mems-talk] contact angle measurement equipment needed

Xiaoguang "Leo" Liu liuxiaoguang at gmail.com
Fri Sep 1 11:27:35 EDT 2006


Thanks Bill
By vacuum bake, yuo mean baking the photoresist in vacuum at low temperature?
Best
Leo

On 9/1/06, Bill Moffat <BMoffat at yieldengineering.com> wrote:
> Try manufacturing your own.  Put a drop of water on a surface shine a
> collimated light say a microscope light at it collect the shadow image
> on a wall and measure the angle. Bill Moffat
>