[mems-talk] Photoresist Hard Bake question
Robert Black
r-black1 at ti.com
Fri Sep 1 14:12:35 EDT 2006
I don't have experience with this resist or at that thickness, but I don't
think the resist should reflow at 85 C. You may try to ramp up to temp on
your hard bake, or maybe a Post exposure bake.
Robert
-----Original Message-----
From: mems-talk-bounces at memsnet.org [mailto:mems-talk-bounces at memsnet.org]
On Behalf Of Xiaoguang "Leo" Liu
Sent: Thursday, August 31, 2006 5:25 PM
To: General MEMS discussion
Subject: [mems-talk] Photoresist Hard Bake question
Dear all
I'm using AZ926 photoressit for a thickness of 20um. However, after
hardbake (85 degree C for 20minutes), the photoresist reflows and does
not maintain the near vertical profile. I wonder if anybody knows
anyway to prevent the reflow of photoresist during the hardbake
process? Thanks a lot.