Greetings,
Yes indeed very smooth .
We use a mask than perform litho, and than we use our microblasting 
technology a stream of ionized particles erodes rapidly the designated areas
hope this helps
walter
----- Original Message ----- 
From: "Xiaoguang "Leo" Liu" <liuxiaoguang at gmail.com>
To: "General MEMS discussion" <mems-talk at memsnet.org>
Sent: Friday, September 01, 2006 8:23 AM
Subject: Re: [mems-talk] Regarding Glass lithography


> Hi Walter
> Could you elaborate a little bit on the "micro/photo machining 
> technology"?
> Do you achieve smooth side wall profile using that kind of tech? Thanks
> Best
> Leo
>
> On 9/1/06, walter essinger <walter at elume.com> wrote:
>> Greetings,
>> did you consider micro/photo machining technology?
>> the 50 M is no problem 200 M is a bit of a challenge..
>> for more info you can contact me
>> engineering at elume.com
>> kind regards
>> walter
>>
>
> 



More information about the MEMS-talk mailing list