[mems-talk] dissolving cured epoxy glue
garber at engr.uconn.edu
garber at engr.uconn.edu
Mon Sep 4 19:23:15 EDT 2006
What kind of epoxy are you using? Duh?
Original Message:
-----------------
From: Mohammad Najmzadeh najmzade at student.chalmers.se
Date: Mon, 4 Sep 2006 21:53:23 +0200 (CEST)
To: mems-talk at memsnet.org
Subject: [mems-talk] dissolving cured epoxy glue
Hello,
I have attached some silicon sensors to an aluminium setup with epoxy glue
and now I want to disconnect them.
I am looking for a way to dissolve this cured epoxy glue.
Heating of it for 3 hours on a hot plate with 200-300 degree C was one
option to dissociate that glue but that was not successful.
Please inform me if you know anything about it.
Kind Regards,
Mohammad Najmzadeh