[mems-talk] floating a thin polymer layer off a substarte
Ning Wu (nwu at Princeton.EDU)
nwu at Princeton.EDU
Wed Sep 6 09:12:23 EDT 2006
Dear all,
I am wondering is there any expert who is familiar the so-called
"floating" method to float a thin polymer layer (e.g. PMMA, PS, etc)
onto water surface from a solid substrate (usually glass)? It was
mentioned many times in literature without any details. Looks like
"trivial" but I did not success. In particular, I am wondering how
larger the film can be floated off and how to do it correctly (like
inclination angle)? Any tips or tricks?
Thanks in advance.
Ning
More information about the MEMS-talk
mailing list