Ti,Cr etc yes lift- off is the best option
regards
walter at elume.com
----- Original Message ----- 
From: "J.J HU" <hjjnst at hotmail.com>
To: <mems-talk at memsnet.org>
Sent: Friday, September 08, 2006 8:09 AM
Subject: [mems-talk] Adhesive layer for gold on oxide and patterning


> Hi all,
> I am trying to put down 300~500nm Au film on Si dioxide as electrodes, and 
> I
> am just wondering what kind of adhesive layer (needs to be electrically
> conductive) should I deposit before Au to improve the adhesion?
>
> And anyone has some good thoughts about how to pattern the gold electrode
> (as well as the adhensive layer)? Will regular lift-off work?
>