Glass frit is not typically patterned by masking.  It is more commonly
patterned by silk-screening.

Best Regards,
Chad Brubaker

EV Group       invent * innovate * implement
Technology - Tel:  480.727.9635, Fax:  480.727.9700  e-mail:
c.brubaker at EVGroup.com, www.EVGroup.com

-----Original Message-----
From: mems-talk-bounces at memsnet.org
[mailto:mems-talk-bounces at memsnet.org] On Behalf Of Kagan Topalli
Sent: Wednesday, September 13, 2006 7:03 AM
To: General MEMS discussion
Subject: [mems-talk] Glass frit coating, masking, and patterning

Hi everbody,
Is there anybody that can advise a reference paper or a book chapter
related 
with glass frit coating, masking, and patterning? Could you please also 
suggest a company that serves glass frit deposition and patterning?