[mems-talk] boron stain
Roger Brennan
roger_brennan at pyramid.net
Mon Sep 25 20:40:57 EDT 2006
A low temperature wet oxidation is the usual fix.
Best of luck,
Roger Brennan
Applications Director
Solecon Labs
770 Trademark Drive
Reno, NV 89521-5926
roger at Solecon.com
775-853-5900 ext 108
-----Original Message-----
From: mems-talk-bounces at memsnet.org
[mailto:mems-talk-bounces at memsnet.org]On Behalf Of Tao
Sent: Monday, September 25, 2006 7:44 AM
To: General MEMS discussion
Subject: [mems-talk] boron stain
Hi,
Does anyone have experience with Borofilm 100? I got some Boron stain on
the doping area after diffusion. It's not soluble in HF ans makes
problems in electric contact.
Can anyone give me some advice on how to clean the stain?