Your gold etch rate seems very slow. We typically etch through several
thousand angstroms in 2-3 minutes. Perhaps your etchant is old or too
dilute. Transene makes a commercial gold etch.
Brad
On 9/25/06 11:54 AM, "ahajjiah at vt.edu" <ahajjiah at vt.edu> wrote:
Dear MEMS,
2) using KI/I2 etch for gold and then using the HF to etch Ti. The etch rate
on this one is very slow, 8A/min. and as a result, my photoresist can't hold
against the etch because it will take me at least 15min to etch through the
gold.