[mems-talk] Etching Ag

Keven_Yu at amat.com Keven_Yu at amat.com
Thu Sep 28 18:30:26 EDT 2006


HCl can be used for wet etching.


Regards,
Keven 


Benyimin Hadad <benyimin at bgu.ac.il> 
Sent by: mems-talk-bounces at memsnet.org 09/28/2006 03:22 PM
To General MEMS discussion <mems-talk at memsnet.org>
Subject [mems-talk] Etching Ag
 
Hello 

I want to know if someone know how to etch Ag , dry and wet .



More information about the MEMS-talk mailing list