[mems-talk] Photoresist with smooth and high resolution sidewall

Bill Moffat BMoffat at yieldengineering.com
Fri Sep 29 12:22:30 EDT 2006


When you say high resolution are you looking for resist with vertical
side walls? 

Bill Moffat, CEO
Yield Engineering Systems, Inc.
2185 Oakland Rd., San Jose, CA  95131
(408) 954-8353


-----Original Message-----
From: mems-talk-bounces at memsnet.org
[mailto:mems-talk-bounces at memsnet.org] On Behalf Of Hsiu-Jen Wang
Sent: Friday, September 29, 2006 1:33 AM
To: mems-talk at memsnet.org
Subject: [mems-talk] Photoresist with smooth and high resolution
sidewall

Hi all,

    I'd like to obtain the information about which type of photoresist
has smooth and high resolution sidewall, whose thickness is 3um~5um.
Could anybody share his/her expeience? Appreciate a lot.