Another question, is there any conductive coating? I'll make an
electric contact.
Thank you.
Best,
Jeff
On 4/25/07, Boris Kobrin <boris_kobrin at appliedmst.com> wrote:
> Hi Jeff,
>
> Yes, you can get >110 deg on PMMA using vapor deposited MVD coatings.
> In-situ deposited adhesion layers will help to attach hydrophobic silanes to
> PMMA material.
>