Hi, You can use powder blasting with a photoresist foil as a mask. MSc. A. (Anil) Agiral *PhD Student * *Mesoscale Chemical Systems Group* University of Twente Faculty of Science and Technology Meander 151 PO Box 217 7500 AE Enschede The Netherlands