[mems-talk] KOH etchant solidification
신현철
cheory58 at naver.com
Mon Aug 13 10:54:04 EDT 2007
Hello everyone,
I want to ask something about KOH etchant to those of you who are familiar with it.
We have KOH etching bench in our cleanroom, in that bench, there is an etchant tank.
So we keep the KOH etchant in the tank, which means it is always exposed to air (even though we have a cover).
One day, when I took a look at it, surface of the etchant were solidified, the surface looked like a milky jelly.
But when I heated up the 90C, now it looked like normal(clean, transparent).
So, I wonder this is normal condition or something wrong with etchant.
Thank you