[mems-talk] selective etching of p type AlGaN over undoped AlGaN?

Yuzhu Li yuzhul at eden.rutgers.edu
Tue Dec 18 13:48:25 EST 2007


Is there a way to selectively etch  p-type AlGaN over undoped AlGaN?
Please give recipe or reference.