gold is a choice. Aluminum may oxidize and may not be suitable.
Best
Leo
On 2/1/07, Sebastian Sosin <s.sosin at ewi.tudelft.nl> wrote:
>
> Does anybody have any idea (hints, published papers, experience) about
> COPPER plating using an ALUMINUM seed layer or some other metal but NOT
> COPPER?
--